Products

Home > Products > Copper > Copper Bar/Rod > W70Cu30 Tungsten-Copper Alloy Bar

W70Cu30 Tungsten-Copper Alloy Bar

Tungsten Copper Bar has a wide range of uses, mainly used to manufacture the contact of high voltage electric switch and high temperature components such as rocket nozzle throat liner and tail rudder, and also used as electrodes for electrical processing, high temperature mold and other occasions requiring high conductivity and high temperature.


Description

General Specifications & Dimensions
Parameter Specification / Range Notes
Common Alloys (UNS) C10100 (OFE), C10200 (OF), C11000 (ETP), C12000 (DLP), C12200 (DHP) C11000 is the most common general-purpose grade; C10200/C10100 are oxygen-free grades for high-conductivity applications
Common Grades (GB) T1, T2, TU1, TU2, TP1, TP2 T2 is the standard grade for high conductivity; TU1/TU2 are oxygen-free grades
Common Grades (JIS) C1100, C1020, C1201, C1220 Japanese Industrial Standard equivalents
Diameter Range 1.0 mm – 200 mm Range varies significantly by application and manufacturing process
Length 100 mm – 6000 mm (standard); custom lengths available Standard lengths vary by supplier; precision cut lengths available
Shape Types Round, Square, Hexagonal, Rectangular Various cross-sections available for different machining and fabrication needs
Applicable Standards GB/T 4423, ASTM B16, JIS H3250, EN 12163, ISO Standards governing chemical composition, mechanical properties, and dimensions
Temper / Hardness Designation M (Soft/Annealed), Y2 (1/2 Hard), Y (Hard), R240, R320, R380 Temper significantly impacts mechanical properties; various designation systems exist across standards.
Manufacturing Process Extruded, Drawn, Cold-Rolled, Continuous Cast, Centrifugal Cast Seamless construction ensures uniform properties and pressure integrity
Surface Finish Mill Finish, Drawn (Bright), Turned, Ground, Polished Finish depends on application requirements and final processing
Purity Range 99.9% (3N) to 99.999% (5N) Purity selection depends on application requirements: 3N for general electrical/thermal, 5N for advanced research and quantum applications.
Alloy Designations & Standards Cross-Reference
UNS No. GB (China) JIS DIN / EN Description
C10100 TU0 C1011 CW009A (Cu-OFE) Oxygen-Free Electronic; 99.99% purity; highest conductivity
C10200 TU1/TU2 C1020 CW008A (Cu-OF) Oxygen-Free; 99.95% purity; no phosphorus deoxidant
C11000 T2 C1100 CW004A (Cu-ETP) Electrolytic Tough Pitch; 99.90% purity; contains ~200-400 ppm oxygen
C12000 TP1 C1201 CW023A (Cu-DLP) Phosphorus Deoxidized, Low Phosphorus (0.004-0.012%)
C12200 TP2 C1220 CW024A (Cu-DHP) Phosphorus Deoxidized, High Phosphorus (0.015-0.040%)
Mechanical Properties (By Temper)
Alloy / Grade Temper Diameter (mm) Tensile Strength (MPa) Yield Strength (MPa)
C11000 M (Soft/Annealed) all 224 54
C11000 Y (Hard) all 314 270
CuZn10 (Brass) R240 4-80 240 150
CuZn10 (Brass) R320 4-40 320 220
CuZn10 (Brass) R380  4-10 380 280

Inquiry Us
  • Submit Reset

Back to list