Home > Products > Copper > Copper Bar/Rod > W75Cu25 Tungsten-Copper Alloy Bar


Tungsten Copper Electrodes are WIDELY used, mainly used in the manufacture of high voltage switch contacts, rocket nozzle throat liner, tail rudder and other high temperature parts, can also be used as electrical processing electrode, high temperature mold and other occasions requiring high conductivity and high temperature.
| General Specifications & Dimensions | ||
| Parameter | Specification / Range | Notes |
| Common Alloys (UNS) | C10100 (OFE), C10200 (OF), C11000 (ETP), C12000 (DLP), C12200 (DHP) | C11000 is the most common general-purpose grade; C10200/C10100 are oxygen-free grades for high-conductivity applications |
| Common Grades (GB) | T1, T2, TU1, TU2, TP1, TP2 | T2 is the standard grade for high conductivity; TU1/TU2 are oxygen-free grades |
| Common Grades (JIS) | C1100, C1020, C1201, C1220 | Japanese Industrial Standard equivalents |
| Diameter Range | 1.0 mm – 200 mm | Range varies significantly by application and manufacturing process |
| Length | 100 mm – 6000 mm (standard); custom lengths available | Standard lengths vary by supplier; precision cut lengths available |
| Shape Types | Round, Square, Hexagonal, Rectangular | Various cross-sections available for different machining and fabrication needs |
| Applicable Standards | GB/T 4423, ASTM B16, JIS H3250, EN 12163, ISO | Standards governing chemical composition, mechanical properties, and dimensions |
| Temper / Hardness Designation | M (Soft/Annealed), Y2 (1/2 Hard), Y (Hard), R240, R320, R380 | Temper significantly impacts mechanical properties; various designation systems exist across standards. |
| Manufacturing Process | Extruded, Drawn, Cold-Rolled, Continuous Cast, Centrifugal Cast | Seamless construction ensures uniform properties and pressure integrity |
| Surface Finish | Mill Finish, Drawn (Bright), Turned, Ground, Polished | Finish depends on application requirements and final processing |
| Purity Range | 99.9% (3N) to 99.999% (5N) | Purity selection depends on application requirements: 3N for general electrical/thermal, 5N for advanced research and quantum applications. |
| Alloy Designations & Standards Cross-Reference | ||||
| UNS No. | GB (China) | JIS | DIN / EN | Description |
| C10100 | TU0 | C1011 | CW009A (Cu-OFE) | Oxygen-Free Electronic; 99.99% purity; highest conductivity |
| C10200 | TU1/TU2 | C1020 | CW008A (Cu-OF) | Oxygen-Free; 99.95% purity; no phosphorus deoxidant |
| C11000 | T2 | C1100 | CW004A (Cu-ETP) | Electrolytic Tough Pitch; 99.90% purity; contains ~200-400 ppm oxygen |
| C12000 | TP1 | C1201 | CW023A (Cu-DLP) | Phosphorus Deoxidized, Low Phosphorus (0.004-0.012%) |
| C12200 | TP2 | C1220 | CW024A (Cu-DHP) | Phosphorus Deoxidized, High Phosphorus (0.015-0.040%) |
| Mechanical Properties (By Temper) | ||||
| Alloy / Grade | Temper | Diameter (mm) | Tensile Strength (MPa) | Yield Strength (MPa) |
| C11000 | M (Soft/Annealed) | all | 224 | 54 |
| C11000 | Y (Hard) | all | 314 | 270 |
| CuZn10 (Brass) | R240 | 4-80 | 240 | 150 |
| CuZn10 (Brass) | R320 | 4-40 | 320 | 220 |
| CuZn10 (Brass) | R380 | 4-10 | 380 | 280 |